| Specification | Test Method | 40/50 | 50/70 | 60/70 | 70/100 | 85/100 | 160/220 | ||||
| Penetration @25°c l00g.5s | ASTM D5 | 40-50 | 50-70 | 60-70 | 70- l 00 | 85- l 00 | 160-220 | ||||
| Ductility @25°c | ASTM Dl 13 | > 100 | > 100 | > 100 | > l 00 | > l 00 | |||||
| Softening point | ASTM D36 | 50-56 | 48-56 | 49-56 | 43-5 l | 42-49 | 35-43 | ||||
| Kinematic Viscosity @l 35°c | ASTM D2170 | 300 min | 300min | 300 min | 230 min | NR | 135min | ||||
| Flash Point | ASTM D92 | 232 min | 232 min | 232 min | 230 min | 230 min | 220min | ||||
| Solubility in (CCL4) | ASTM D2042 | > 99 | > 99 | > 99 | > 99 | > 99 | > 99 | ||||
| Specific Gravity @25°c | ASRM D70 | l.01- 1.06 | 1.01-1.06 | 1.01- 1.06 | 1 | 1.0 l- 1.06 | 1.01 | 1- 1.06 | |||
| Ash Content W% | ASTM D482 | NR | NR | NR | NR | NR | |||||
| Water Content | ASTM D95 | < 0.2 | < 0.2 | < 0.2 | Nil | N | il | ||||
| Loss on Heating W% | ASTM D6 | < 0.5 | < 0.5 | < 0.5 | <0.8 | <l | l.0max | ||||
| Retained Penetration (T.F.O.T) | ASTM D5 | > 30 | 40min | > 54 | > 56 | > 47 | 70min | ||||
| Retained Ductility @25°c | ASTM Dl 13 | > 25 | 50min | > 50 | > 75 | > 75 | |||||
| Increase in softening point | ASTM D36 | <l l | <10 | l l .0 max | |||||||
| Test | Test Method | VG-10 | VG-20 | VG-30 | VG-40 |
| Absolute Viscosity @60Qc, Poises (min) | ASTM D-2171 | 800 | 1600 | 2400 | 3200 |
| Kinematic Viscosity @l 35Qc, c5t (min) | ASTM D-2170 | 250 | 300 | 350 | 400 |
| Flash Point (Cleveland Open-Cup), Qc (min) | ASTM D-92 | 220 | 220 | 220 | 220 |
| Solubility in Trichloroethylene, % (min) | ASTM D-20-40 | 99 | 99 | 99 | 99 |
| Softening Point, Ring & Ball, Qc | ASTM D-36 | 40 | 45 | 47 | 50 |
| Penetration @25°c, 0.1mm, l 00gr, 5sec | 5 | 80- l 00 | 80 | 50-70 | 40-60 |
| Specific Gravity @27/27Qc (min) | ASTM D-70 | 0.99 | 0.99 | 0.99 | 0.99 |
| Tests on residue from TFOT: | |||||
| l) Viscosity ratio @60Qc (max) | ASTM D-2171 | 4.0 | 4.0 | 4.0 | 4.0 |
| 2) Ductility @25°c, cm, after TFOT (min) | ASTM D-113 | 75 | 50 | 40 | 25 |
| Specification | Test Method | 40/50 | 50/70 | 60/70 | 70/100 | 85/100 | 160/220 | ||||
| Penetration @25°c l00g.5s | ASTM D5 | 40-50 | 50-70 | 60-70 | 70- l 00 | 85- l 00 | 160-220 | ||||
| Ductility @25°c | ASTM Dl 13 | > 100 | > 100 | > 100 | > l 00 | > l 00 | |||||
| Softening point | ASTM D36 | 50-56 | 48-56 | 49-56 | 43-5 l | 42-49 | 35-43 | ||||
| Kinematic Viscosity @l 35°c | ASTM D2170 | 300 min | 300min | 300 min | 230 min | NR | 135min | ||||
| Flash Point | ASTM D92 | 232 min | 232 min | 232 min | 230 min | 230 min | 220min | ||||
| Solubility in (CCL4) | ASTM D2042 | > 99 | > 99 | > 99 | > 99 | > 99 | > 99 | ||||
| Specific Gravity @25°c | ASRM D70 | l.01- 1.06 | 1.01-1.06 | 1.01- 1.06 | 1 | 1.0 l- 1.06 | 1.01 | 1- 1.06 | |||
| Ash Content W% | ASTM D482 | NR | NR | NR | NR | NR | |||||
| Water Content | ASTM D95 | < 0.2 | < 0.2 | < 0.2 | Nil | N | il | ||||
| Loss on Heating W% | ASTM D6 | < 0.5 | < 0.5 | < 0.5 | <0.8 | <l | l.0max | ||||
| Retained Penetration (T.F.O.T) | ASTM D5 | > 30 | 40min | > 54 | > 56 | > 47 | 70min | ||||
| Retained Ductility @25°c | ASTM Dl 13 | > 25 | 50min | > 50 | > 75 | > 75 | |||||
| Increase in softening point | ASTM D36 | <l l | <10 | l l .0 max | |||||||

| Test | Test Method | VG-10 | VG-20 | VG-30 | VG-40 |
| Absolute Viscosity @60Qc, Poises (min) | ASTM D-2171 | 800 | 1600 | 2400 | 3200 |
| Kinematic Viscosity @l 35Qc, c5t (min) | ASTM D-2170 | 250 | 300 | 350 | 400 |
| Flash Point (Cleveland Open-Cup), Qc (min) | ASTM D-92 | 220 | 220 | 220 | 220 |
| Solubility in Trichloroethylene, % (min) | ASTM D-20-40 | 99 | 99 | 99 | 99 |
| Softening Point, Ring & Ball, Qc | ASTM D-36 | 40 | 45 | 47 | 50 |
| Penetration @25°c, 0.1mm, l 00gr, 5sec | 5 | 80- l 00 | 80 | 50-70 | 40-60 |
| Specific Gravity @27/27Qc (min) | ASTM D-70 | 0.99 | 0.99 | 0.99 | 0.99 |
| Tests on residue from TFOT: | |||||
| l) Viscosity ratio @60Qc (max) | ASTM D-2171 | 4.0 | 4.0 | 4.0 | 4.0 |
| 2) Ductility @25°c, cm, after TFOT (min) | ASTM D-113 | 75 | 50 | 40 | 25 |